Differential scanning calorimeter DSC-7

Domaine d'application
- Physical and chemical analysis
Spécialité
- Differential scanning calorimetry (DSC)
Description
- This machine serves to determine the phase changes occuring in substances as temperatures rise.
- It is useful for analysis of precipitate formation during forging as well as texture formation.