Spécialité d’équipement Differential scanning calorimetry (DSC)
- Power-compensation differential scanning calorimeter able to reach 725 °C.
- Power-compensation differential scanning calorimeter at temperatures up to 725 °C.
- This machine serves to determine the phase changes occuring in substances as temperatures rise.
- It is useful for analysis of precipitate formation during forging as well as texture formation.
- Netzch STA 449 F3 Jupiter
- Differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA)
- Maximum temperature: 1650 °C